Fig 1.

(a) Sample schematic [units in mm] (b) Side view of stack with bolt arrangement prior to cutting.

More »

Fig 1 Expand

Fig 2.

SEM results (×250 magnification) secondary electron 15kV for layers 1 (top) to 7 (bottom).

More »

Fig 2 Expand

Fig 3.

SEM results of cut edge (×500 magnification) secondary electron 15kV for layers 1 (top) to 6 (bottom).

More »

Fig 3 Expand

Fig 4.

Stack 1, Layer 1.

SEM ×2000 Zoom at cut edge.

More »

Fig 4 Expand

Fig 5.

SEM results of mid-section (away from cut) (×500 magnification) secondary electron 15kV.

More »

Fig 5 Expand

Fig 6.

Layers joined in various laser cutting stack sizes (Black loose, Red joined to layer beneath).

More »

Fig 6 Expand

Fig 7.

B-H (Flux Density & Magnetizing Force) curve for samples produced by laser cutting stacks.

More »

Fig 7 Expand

Fig 8.

Absolute losses of laminations.

More »

Fig 8 Expand

Fig 9.

Percentage increase in losses of laminations after different cutting procedures.

More »