Table 1.

Chemical composition of the oxo-biodegradable plastic before and after 120 days of sunlight exposure.

More »

Table 1 Expand

Figure 1.

Mechanical properties of the oxo-biodegradable plastic before and after 30, 60, 90 or 120 days of sunlight exposure.

*Value was multiplied by 10, ** Value was divided by 10.

More »

Figure 1 Expand

Figure 2.

Spectrum of Fourier transform infrared spectroscopy of oxo-biodegradable plastic before (Ox0duv) and after 120 days of sunlight exposure (0x120duv).

More »

Figure 2 Expand

Figure 3.

Scanning electron microscopy of oxo-biodegradable plastic before (Ox0duv) and after 30 (Ox30duv), 60 (Ox60duv), 90 (Ox90duv) and 120 days (Ox120duv) of sunlight exposure.

More »

Figure 3 Expand

Figure 4.

Scanning electron microscopy of Pleurotus ostreatus hyphae grown on the surface of oxo-biodegradable plastic.

White arrows and white circles denote the septa and adhesion hyphae, respectively.

More »

Figure 4 Expand

Figure 5.

Respiratory activity of Pleurotus ostreatus, following 90 days of growth, before (Ox0duv) and after 30 (Ox30duv), 60 (Ox60duv), 90 (Ox90duv) and 120 days (Ox120duv) of sunlight.

*Exponential equation significance (p<0.05). There were no differences between Ox30duv and Ox60duv or Ox90duv and Ox120duv.

More »

Figure 5 Expand

Figure 6.

Dry mass of the substrates, used for 90 days of Pleurotus ostreatus growth, before (Ox0duv) and after 30 (Ox30duv), 60 (Ox60duv), 90 (Ox90duv) or 120 days (Ox120duv) of sunlight.

More »

Figure 6 Expand

Table 2.

Mechanical properties of oxo-biodegradable plastic before and after 30, 60 or 90 days of incubation with Pleurotus ostreatus.

More »

Table 2 Expand

Figure 7.

Scanning electron microscopy of oxo-biodegradable plastic before and after 120 days of sunlight and after 30, 60 and 90 days of incubation with Pleurotus ostreatus.

More »

Figure 7 Expand

Figure 8.

X-ray diffraction of oxo-biodegradable plastic before exposure to sunlight (A) and after 120 days of sunlight and 90 days of incubation.

The small red points represent titanium.

More »

Figure 8 Expand

Table 3.

Fourier transform infrared spectroscopy spectra of chemical alterations in oxo-biodegradable plastic after 30, 60 and 90 days of incubation with Pleurotus ostreatus.

More »

Table 3 Expand

Figure 9.

Bands of nifH gene from Pleurotus ostreatus mycelium.

Numbers represent the order of the bands (see table 4). M = marker.

More »

Figure 9 Expand

Table 4.

Comparison of the nifH gene sequence from Pleurotus ostreatus and sequences of similar genes deposited in GenBank.

More »

Table 4 Expand