Skip to main content
Advertisement
Browse Subject Areas
?

Click through the PLOS taxonomy to find articles in your field.

For more information about PLOS Subject Areas, click here.

< Back to Article

Figure 1.

(a) Schematic illustration of the experiment setup. (b) Schematic of the impact process to the layered glass. (c) View of glass sample before and after impact.

More »

Figure 1 Expand

Figure 2.

Images depicting the crack growth on the two glass layers (V = 3.7 m/s).

More »

Figure 2 Expand

Figure 3.

Radial crack velocity vs. crack length with different radial crack number (V = 3.7 m/s).

More »

Figure 3 Expand

Figure 4.

Selected sequence of images depicting the crack patterns on both glass layers at the loading speed vd = 3.7 m/s, with PVB thickness h = 0.76 mm.

More »

Figure 4 Expand

Figure 5.

Crack length on the inner glass layer vs. radial crack number (V = 2.42 m/s).

More »

Figure 5 Expand