Figure 1.

X-ray structure of ligand 5. Hydrogen atoms are omitted for clarity.

More »

Figure 1 Expand

Figure 2.

Size-exclusion chromatogram for Sample 6.

More »

Figure 2 Expand

Table 1.

Bulk cobalt mediated radical polymerization of methyl methacrylate in the presence of dinuclear complex 4 and complex 5.

More »

Table 1 Expand

Figure 3.

Size-exclusion chromatograms for Sample 1–3.

More »

Figure 3 Expand

Figure 4.

Size-exclusion chromatograms for Sample 4–7.

More »

Figure 4 Expand

Figure 5.

Dependence of PMMA molar mass Mn on monomer conversion Z for bulk polymerization of MMA at 80°C (for the primary constituent of the obtained PMMA).

[MMA]/[Co(II)] = 600 (Table 1). (□ complex 4, • complex 5)

More »

Figure 5 Expand

Figure 6.

Time dependence of ln([M]0/[M]) for the bulk polymerization of MMA at 80°C (for the primary constituent of the obtained PMMA).

[MMA]/[Co(II)] = 600 (Table 1). [M]0 and [M] are the MMA concentration at times 0 and t, respectively. (□ complex 5; ▪complex 4)

More »

Figure 6 Expand

Figure 7.

Size-exclusion chromatogram for the macroinitiator and block copolymer.

More »

Figure 7 Expand